Polymer Property : Shielding Effectiveness = 130 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness >= 130 dB

@Frequency 1.00e+7 Hz
>= 130 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Waveguide Gaskets 877 Conductive Silicone Elastomer Gasket
Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W..
Shielding Effectiveness >= 130 dB

@Frequency 1.00e+7 Hz
>= 130 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer
Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se..
Shielding Effectiveness >= 130 dB

@Frequency 1.00e+7 Hz
>= 130 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer
Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se..
Shielding Effectiveness 130 dB

@Frequency 1.00e+7 Hz
130 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer
Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi..
Shielding Effectiveness 130 dB

@Frequency 1.00e+7 Hz
130 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Tecknit Consil®-II 842 Molded Silver-Filled Silicone Elastomer
Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi..
Shielding Effectiveness >= 130 dB

@Frequency 1.00e+7 Hz
>= 130 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation..
Shielding Effectiveness >= 130 dB

@Frequency 1.00e+7 Hz
>= 130 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by ..
Shielding Effectiveness >= 130 dB

@Frequency 1.00e+7 Hz
>= 130 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Waveguide Gaskets 873 Conductive Silicone Elastomer Gasket