Electrical Properties Metric English Comments
Shielding Effectiveness 101 dB

@Frequency 1.00e+8 Hz
101 dB

@Frequency 1.00e+8 Hz
E-Field
P & P Technology Conductive Elastomer
Nickel Graphite particlesInformation provided by P & P Technology
Shielding Effectiveness 101 dB

@Frequency 2.00e+9 Hz
101 dB

@Frequency 2.00e+9 Hz
Mil-G-83528/Mil std 285
P & P Technology EC-H Silver Copper Loaded Fluorosilicone
P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer exc..
Shielding Effectiveness 101 dB

@Frequency 2.00e+9 Hz
101 dB

@Frequency 2.00e+9 Hz
Mil-G-83528/Mil std 285
P & P Technology EC-H Silver Copper Loaded Silicone
P & P Technology material reference EC-H is a printing grade silicone elastomer with a Silver/Copper conductive filler and is Tan in color. The material is specially compounded to offer excellent p..