Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 75 sec | 75 sec | ASTM D495 |
Covestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Arc Resistance | 75 sec | 75 sec | ASTM D495 |
Covestro Petlon® 4835 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Arc Resistance | 75 sec @Thickness 3.17 mm |
75 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP130HF Glass Fabric Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens.. |
|||
Arc Resistance | 75 sec @Thickness 3.17 mm |
75 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |