Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 65 sec | 65 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |
|||
Arc Resistance | 65 sec | 65 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
Arc Resistance | 65 sec @Thickness 3.17 mm |
65 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP613 Paper Base Laminate Description: NP613 is constructed from electrical grade of kraft paper and a specially modified epoxy resin system. It is designed to be used in tap changers, coil support plates and terminal panels.. |
|||
Arc Resistance | 65 sec | 65 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Arc Resistance | 65 sec | 65 sec | IPC TM-650 2.5.1 |
Arlon 45N Multifunctional Epoxy Laminate and Prepreg Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi.. |
|||
Arc Resistance | 65 sec | 65 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |
|||
Arc Resistance | 65 sec | 65 sec | IPC TM-650 2.5.1 |
Arlon 44N Multifunctional Microdispersed Ceramic Filled Epoxy-Fiberglass Prepreg Arlon 44N is a high resin content multifunctional (175°C) epoxy prepreg system with a proprietary microdispersed ceramic filler system. 44N is engineered for the filling of clearance holes in thi.. |