Polymer Property : Arc Resistance = 50 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 50 sec
50 sec
ASTM D495
Plenco 50240 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
Arc Resistance 50 sec
50 sec
ASTM D495
Plenco 51240 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
Arc Resistance 50 sec
50 sec
ASTM D495
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)  (discontinued **)
Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl..
Arc Resistance >= 50 sec
>= 50 sec
Test Terminated at 50 sec.; ASTM D495
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Arc Resistance >= 50 sec
>= 50 sec
Test Terminated at 50 sec.; ASTM D495
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Arc Resistance >= 50 sec
>= 50 sec
ASTM D495
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Arc Resistance >= 50 sec
>= 50 sec
ASTM D495
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Arc Resistance 50 sec
50 sec
ASTM D495
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac
XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu..
Arc Resistance >= 50 sec
>= 50 sec
ASTM D495
CPC - Vycom FLAMETEC™ KYTEC® PVDF
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e..
Arc Resistance >= 50 sec
>= 50 sec
ASTM D495
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Arc Resistance 50 sec
50 sec
ASTM D495
Gharda Chemicals Gafone™ B2315GF Polysupersulfone (PSS)  (discontinued **)
Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical..
Arc Resistance 50 sec
50 sec
ASTM D495
Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound  (discontinued **)
Polyphenylene Sulfide CompoundRyton® PR09-60 is pelletized unfilled high molecular weight polyphenylene sulfide resin suitable for extrusion or injection molding.Comments: Test specimen molding con..
Arc Resistance 50 sec
50 sec
ASTM D495
Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound, Annealed 2 hours at 200°C  (discontinued **)&l
Polyphenylene Sulfide CompoundRyton® PR09-60 Annealed 2 hours at 200°C is pelletized unfilled high molecular weight polyphenylene sulfide resin suitable for extrusion or injection molding.Comments..
Arc Resistance 50 sec
50 sec
ASTM D495
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)  (discontinued **)
Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical..