Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Arc Resistance = 200 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Network Polymers Kepital® F10-02
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Network Polymers Kepital® F20-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Network Polymers Kepital® F20-52
Description: Natural Acetal Copolymer, Weather Resistance GradeInformation provided by Network Polymers Inc.
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Network Polymers Kepital® F30-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Network Polymers Kepital® F40-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Kolon Kocetal® VT701 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Arc Resistance 200 sec

@Thickness 3.17 mm
200 sec

@Thickness 0.125 in
ASTM D495
Industrial Laminates/Norplex NP159 Synthetic Fabric  (discontinued **)
Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit..
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Arc Resistance 200 sec
200 sec
ASTM D495
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound
Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information ..
Arc Resistance >= 200 sec
>= 200 sec
ASTM D495
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin
Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor ..
Arc Resistance 200 sec
200 sec
Dow Corning 5-8601 FLUOROSILICONE LSR, KIT
Fluorosilicone rubber designed for liquid injection moldingInformation provided by Dow Corning
Arc Resistance 200 sec
200 sec
ASTM D495
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound
SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp..
Copyright © lookpolymers.com All Rights Reserved