Polymer Property : Arc Resistance = 195 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 195 sec
195 sec
ASTM D495
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity
Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical
Arc Resistance 195 sec
195 sec
ASTM D495
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity
Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical
Arc Resistance 195 sec
195 sec
ASTM D495
LG Chemical LUMID GP1300A(W) PA6, High Viscosity
Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical
Arc Resistance 195 sec
195 sec
ASTM D495
LG Chemical LUMID GP1300AP PA6, Plasticized
Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical
Arc Resistance 195 sec
195 sec
ASTM D495
LG Chemical LUMID HI1102A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
Arc Resistance 195 sec
195 sec
ASTM D495
LG Chemical LUMID HI1202A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
Arc Resistance 195 sec
195 sec
Tungsten electrode; ASTM D495
E-Polymers TEKAMID® TB120L NCR , High Crystallinity PA6, DAM
Precise injection, high crystallinityInformation provided by E-Polymers Co. Ltd.
Arc Resistance 195 sec
195 sec
Tungsten electrode; ASTM D495
E-Polymers TEKAMID® TB120L Lubricated PA6, DAM
LubricatedInformation provided by E-Polymers Co. Ltd.
Arc Resistance 195 sec
195 sec
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester
BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re..