Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 177 sec | 177 sec | ASTM D495 |
Plenco 4349 Phenolic, Granular, Compression Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Arc Resistance | 177 sec | 177 sec | ASTM D495 |
Plenco 7507 Phenolic, Granular, Injection Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Arc Resistance | 177 sec | 177 sec | ASTM D495 |
Plenco 4504 Phenolic, Granular, Injection Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |