Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 10000 - 1.0e+6 ohm | 10000 - 1.0e+6 ohm | IEC 60093 |
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data) Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l.. |