Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data) Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data) TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Surface Resistivity per Square | >= 1.0e+12 ohm | >= 1.0e+12 ohm | IEC 60093 |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |