Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+16 ohm | >= 1.00e+16 ohm | EOS/ESD S11.11 |
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Surface Resistivity per Square | >= 1.00e+16 ohm | >= 1.00e+16 ohm | ASTM D257 |
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
GEHR Plastics Ultem 2300 PEI-30 GF 30% Glass Fiber Reinforced
(discontinued **) Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and great resistance. It's unique torque strength permits the econom.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman Eastar EN052 Polyester Eastar Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman Sahara Film Sahara Films are developed for use in applications where increased temperature resistance is desired.Applications/UsesHigh temperature printable films |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent fle.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm @Temperature 23.0 °C |
1.00e+16 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT 4011 Polyimide, Yellow (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |