Polymer Property : Surface Resistivity per Square = 1.00e+12 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+10 - 1.00e+12 ohm
1.00e+10 - 1.00e+12 ohm
EOS/ESD S11.11
Quadrant EPP Semitron® ESd 520HR (ASTM Product Data Sheet)
Surface Resistivity per Square 1.00e+10 - 1.00e+12 ohm
1.00e+10 - 1.00e+12 ohm
EOS/ESD S11.11
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet)
Surface Resistivity per Square 1.00e+10 - 1.00e+12 ohm
1.00e+10 - 1.00e+12 ohm
ASTM D648
Techmer ES Electrafil® ABS-1200/SD/FR BL ABS
Surface Resistivity per Square 1.00e+11 - 1.00e+12 ohm

@Temperature 23.0 °C
1.00e+11 - 1.00e+12 ohm

@Temperature 73.4 °F
IEC 60093
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Surface Resistivity per Square 1.00e+7 - 1.00e+12 ohm
1.00e+7 - 1.00e+12 ohm
ASTM D257
Ensinger Hydel® PC-P ESD Polycarbonate (PC)
HYDEL® PC-P ESD polycarbonate is a static dissipative thermoplastic product containing carbon powder. This material has good stiffness, excellent dimensional ability, and low outgassing properties..
Surface Resistivity per Square 1.00e+9 - 1.00e+12 ohm
1.00e+9 - 1.00e+12 ohm
ASTM D257
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical..
Surface Resistivity per Square 1.00e+10 - 1.00e+12 ohm
1.00e+10 - 1.00e+12 ohm
EOS/ESD S11.11
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet)