Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+11 ohm | 1.00e+11 ohm | |
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
Surface Resistivity per Square | <= 1.00e+11 ohm | <= 1.00e+11 ohm | VDE 0303 |
GEHR Plastics POM-ESD Acetal, Antistatic Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Surface Resistivity per Square | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer Description: IStat-Rite® E-1150 blend is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1150 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy sys.. |
|||
Surface Resistivity per Square | 1.00e+11 ohm | 1.00e+11 ohm | 50% RH; ASTM D257 |
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+11 - 1.00e+12 ohm @Temperature 23.0 °C |
1.00e+11 - 1.00e+12 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Surface Resistivity per Square | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Diamond Polymers TR 5000 AS/P Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc. |
|||
Surface Resistivity per Square | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Clariant Renol PA1SP0004 Nylon 66, High Impact Modified, ESD Data provided by Clariant Masterbatches |
|||
Surface Resistivity per Square | 1.00e+11 ohm | 1.00e+11 ohm | Non-adhesive side; ASTM D257 |
3M 4504 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | 1.00e+11 ohm | 1.00e+11 ohm | Adhesive side; ASTM D257 |
3M 4508 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |