Polymer Property : Surface Resistivity per Square = 0.0030 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.0030 ohm
<= 0.0030 ohm
[ohm/in<sup>2<sup>]; <.0005 ohm/cm<sup>2</sup>; MIL-STD-202C
Parker Chomerics CHO-FOIL CCE Shielding Tape
Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti..
Surface Resistivity per Square <= 0.0030 ohm
<= 0.0030 ohm
[ohm/in<sup>2<sup>]; <.0005 ohm/cm<sup>2</sup>; MIL-STD-202C
Parker Chomerics CHO-FOIL CCH Shielding Tape
Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti..
Surface Resistivity per Square <= 0.0030 ohm
<= 0.0030 ohm
[ohm/in<sup>2<sup>]; <.0005 ohm/cm<sup>2</sup>; MIL-STD-202C
Parker Chomerics CHO-FOIL CCK Shielding Tape
Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum..
Surface Resistivity per Square <= 0.0030 ohm
<= 0.0030 ohm
Lord Adhesives Metech 3255 Silver Conductor
This conductor composition is a silver bearing paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The ..
Surface Resistivity per Square <= 0.0030 ohm
<= 0.0030 ohm
Lord Adhesives Metech 3288 Silver Conductor
This product is a silver paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The fired film forms a hig..
Surface Resistivity per Square 0.0030 - 0.0090 ohm

@Thickness 0.0100 mm
0.0030 - 0.0090 ohm

@Thickness 0.000394 in
cured
Gwent Electronic Materials C2121119D9 Nanocopper based Paste
This product is a nanocopper based paste that is designed for flat bed screens. The product is compatible with printing on PET substrates such as the DuPont Melinex ST-505. Produced using nano-par..