Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 280 V | 280 V | IEC 60112 |
Polyplastics Duranex® 6300T Polybutylene Terephthalate (PBT), Low friction, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Comparative Tracking Index | 280 V | 280 V | IEC 60112 |
Polyplastics Duranex® 6302T Polybutylene Terephthalate (PBT), Low friction, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Comparative Tracking Index | 280 V | 280 V | IEC test |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |