Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 150 - 275 V | 150 - 275 V | Average value: 225 V Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Comparative Tracking Index | 150 - 275 V | 150 - 275 V | Average value: 206 V Grade Count:38 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Comparative Tracking Index | 125 - 275 V | 125 - 275 V | Average value: 145 V Grade Count:39 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |