Polymer Property : Comparative Tracking Index = 195 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Comparative Tracking Index 195 V
195 V
VDE 0303-P1, IEC 112
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber
Characteristics: 10% glass fibre filled, good mechanical properties
Comparative Tracking Index 195 V
195 V
VDE 0303-P1, IEC 112
EPICHEM Epilon G4-PC 20% GF Polycarbonate, 20% Glass Fiber
Characteristics: 20% glass fibre filled, excellent mechanical properties