Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 8.80e+14 ohm-cm @Temperature 25.0 °C |
8.80e+14 ohm-cm @Temperature 77.0 °F |
|
Abatron AboCast 8-8/Abocure 8-8 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 135 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)... |