Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 0.000115 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000115 ohm-cm

@Temperature 538 °C
0.000115 ohm-cm

@Temperature 1000 °F
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 600 °C
0.000115 ohm-cm

@Temperature 1110 °F
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 700 °C
0.000115 ohm-cm

@Temperature 1290 °F
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 800 °C
0.000115 ohm-cm

@Temperature 1470 °F
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 900 °C
0.000115 ohm-cm

@Temperature 1650 °F
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 93.0 °C
0.000115 ohm-cm

@Temperature 199 °F
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy
INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 1000 °C
0.000115 ohm-cm

@Temperature 1830 °F
Temperature resistance factor (F) =1.062
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 600 °C
0.000115 ohm-cm

@Temperature 1110 °F
Temperature resistance factor (F) =1.068
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Temperature resistance factor (F) =1.065
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 800 °C
0.000115 ohm-cm

@Temperature 1470 °F
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Electrical Resistivity 0.000115 ohm-cm

@Temperature 500 °C
0.000115 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Copyright © lookpolymers.com All Rights Reserved