Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000101 ohm-cm @Temperature -73.0 °C |
0.000101 ohm-cm @Temperature -99.4 °F |
|
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |