Electrical Properties Metric English Comments
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, aged 1000 hours at 982°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, all-weld metal, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, mill annealed
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000930 ohm-cm

@Temperature 200 °C
0.0000930 ohm-cm

@Temperature 392 °F
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..