Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 9.00e+15 ohm | >= 9.00e+15 ohm | ASTM D257 |
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Surface Resistance | 9.00e+15 ohm | 9.00e+15 ohm | IEC 60093 |
Polyplastics Duracon® TR-20 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Surface Resistance | 9.00e+15 ohm | 9.00e+15 ohm | IEC 60093 |
Polyplastics Duranex® 3105 Polybutylene Terephthalate (PBT), Standard, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |