Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 8.95e+13 ohm | 8.95e+13 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East) Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating .. |