Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 6.00e+10 ohm | 6.00e+10 ohm | |
LE Phenolic Laminate Linen based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many st.. |
|||
Surface Resistance | 6.00e+10 ohm | 6.00e+10 ohm | Moisture Resistance; MIL-I-46058C |
Humiseal 1B31 Acrylic Conformal Coating Humiseal 1B31 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C ApprovedPasses thermal shock test (MI.. |
|||
Surface Resistance | 6.00e+10 ohm | 6.00e+10 ohm | Moisture Resistance; MIL-I-46058C |
Humiseal 1B31LSE Acrylic Conformal Coating Humiseal 1B31LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C Approval PendingPasses thermal sho.. |
|||
Surface Resistance | 6.00e+10 ohm | 6.00e+10 ohm | Moisture Resistance; MIL-I-46058C |
Humiseal 1C55 Silicone Conformal Coating Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Surface Resistance | 6.00e+10 ohm | 6.00e+10 ohm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |