Polymer Property : Surface Resistance = 5.00e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 5.00e+14 ohm
5.00e+14 ohm
IEC 60093
DSM Akulon® F232-DH Nylon 6 (European Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Surface Resistance >= 5.00e+14 ohm
>= 5.00e+14 ohm
500V; Ø 93x3mm; IEC 93
SYNTHOS Krasten® 662E High Impact Polystyrene
High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa..
Surface Resistance 5.00e+14 ohm
5.00e+14 ohm
IEC 93
Solvay Technyl® A 205F Nylon 66, EH0
Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula..
Surface Resistance 5.00e+14 ohm
5.00e+14 ohm
IEC 60093
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Surface Resistance 5.00e+14 ohm
5.00e+14 ohm
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive
Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e..
Surface Resistance 5.00e+14 ohm
5.00e+14 ohm
IEC 60093
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Surface Resistance 5.00e+14 ohm
5.00e+14 ohm
IEC 60093
DSM Akulon® K223-TP4 Impact Modified Nylon 6 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Surface Resistance 5.00e+14 ohm
5.00e+14 ohm
C96/35/90; IPC TM-650 2.5.17.1
Arlon 35N Fast Cure Polyimide Laminate and Prepreg
High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi..
Surface Resistance >= 5.00e+14 ohm
>= 5.00e+14 ohm
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..
Surface Resistance >= 5.00e+14 ohm
>= 5.00e+14 ohm
ASTM D257
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..
Surface Resistance 5.00e+14 ohm
5.00e+14 ohm
IEC 60093
DSM Akulon® K223-TP4 (Cond.) Impact Modified Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Surface Resistance >= 5.00e+14 ohm
>= 5.00e+14 ohm
500V; Ø 93x3mm; IEC 93
SYNTHOS Krasten® 336M High Impact Polystyrene
Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos.
Surface Resistance >= 5.00e+14 ohm
>= 5.00e+14 ohm
500V; Ø 93x3mm; IEC 93
SYNTHOS Krasten® 552M High Impact Polystyrene
High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i..