Electrical Properties Metric English Comments
Surface Resistance 4.70e+14 ohm

@Thickness 1.22 mm
4.70e+14 ohm

@Thickness 0.0480 in
ASTM D257
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid)