Polymer Property : Surface Resistance = 350 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 350 - 2.50e+16 ohm
350 - 2.50e+16 ohm
Average value: 6.57e+14 ohm Grade Count:78
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Surface Resistance 350 ohm
350 ohm
LATI Latistat 66-06 PA66
Dissipative product based on Polyamide 66 (PA66). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..