Polymer Property : Surface Resistance = 2500 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 2500 - 4.00e+14 ohm
2500 - 4.00e+14 ohm
Average value: 2.37e+13 ohm Grade Count:46
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Surface Resistance 2500 ohm
2500 ohm
LATI Latiohm 66-04 PD01 G/25-V0CT1 PA66, 25% Glass Fiber Reinforced, Flame Retardant
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;..
Surface Resistance 2500 ohm
2500 ohm
ASTM D257
Techmer ES Electrablend® ABS CF40 BK 40% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.