Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2000 - 1.00e+16 ohm | 2000 - 1.00e+16 ohm | Average value: 8.84e+14 ohm Grade Count:35 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Surface Resistance | 2000 ohm | 2000 ohm | |
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Surface Resistance | 2000 ohm | 2000 ohm | |
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Surface Resistance | 2000 ohm | 2000 ohm | |
LATI Latiohm 87/28-05 PD01 G/10 PC, 10% Glass Fiber Reinforced Semiconductive/dissipative product based on Polycarbonate (PC). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Surface Resistance | 2000 ohm | 2000 ohm | IEC 60093 |
Barlog Plastics KEBAFORM C 901 CB POM Copolymer unreinforced, electr. conductive POMInformation provided by BARLOG plastics GmbH. |