Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+13 - 2.00e+16 ohm | 1.00e+13 - 2.00e+16 ohm | Average value: 2.62e+15 ohm Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Surface Resistance | 1.00e+12 - 2.00e+16 ohm | 1.00e+12 - 2.00e+16 ohm | Average value: 5.79e+15 ohm Grade Count:13 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 1.00e+6 - 2.00e+16 ohm | 1.00e+6 - 2.00e+16 ohm | Average value: 2.84e+15 ohm Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |