Electrical Properties Metric English Comments
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
ASTM D257
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
ASTM D257
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade
Amber pelletsInformation provided by Infinite Polymer System II.
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
ASTM D257
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
IEC 60093
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade
Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles.
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
500V; Ø 93x3mm; IEC 60093
SYNTHOS Forsan® 548 Acrylonitrile Butadiene Styrene (ABS)
Easy flow, glossy, impact resistant.Applications: General purposeVarious technical parts, household appliances, hobby and office equipment, etc.Synthos was formerly known as Kaucuk. All information ..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
ASTM D257
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
IEC 60093
Polyplastics Duranex® 303RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
IEC 60093
Polyplastics Duranex® 313RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
IEC 60093
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
IEC 60093
Polyplastics Duranex® 3306 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
IEC 60093
Polyplastics Duranex® 3400 Polybutylene Terephthalate (PBT), Standard, 40% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
Loctite® 3534 Glob Top Encapsulant
COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
ASTM D257
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
ASTM D257
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
Average value: 2.00e+16 ohm Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
IEC 60093
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
Surface Resistance 2.00e+16 ohm
2.00e+16 ohm
IEC 60093
Polyplastics Duracon® GH-25 Acetal Co-polymer (POM), GF 25% reinforced, High strength, High rigidity
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..