Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.00e+11 ohm | 2.00e+11 ohm | |
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Surface Resistance | 2.00e+11 ohm | 2.00e+11 ohm | |
Sanyo PELESTAT® NC6321 ABS (12wt%) PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a va.. |
|||
Surface Resistance | 2.00e+11 ohm | 2.00e+11 ohm | ASTM D249 |
PlastxWorld CEVIAN® E10 Inherently Static Dissipative ABS Inherently Static Dissipative ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Surface Resistance | 2.00e+11 ohm | 2.00e+11 ohm | ASTM D257 |
Tipco Tipcolite® THD 111 Phenolic Compound, Short Glass Fibers & Minerals, Medium -Soft Flow & High Strength Medium -Soft Flow Phenolic Compound, Reinforced with Short Glass Fibres & MineralsApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, T.. |