Electrical Properties Metric English Comments
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D 257
SABIC Innovative Plastics LNP Faradex ES003DE PEI
LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX ES003E PEI
LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding.
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX WX94736 PBT
LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel.
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS
LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive.
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS
LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive.
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS
LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC
LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive.
Surface Resistance 2.0 - 5.0 ohm
2.0 - 5.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DD0001I PC
LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DD0009E PC
LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DE004ER PC
LNP* STAT-KON* DE004ER is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added featuresof this material include: Electrically Conductive, Easy Molding, Mold Release.
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DX98477 PC
LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON FX98501 PE
LNP* STAT-KON* FX98501 is a compound based on Polyethylene resin containing Proprietary Fillers. Added feature of this material is: Electrically Conductive.
Surface Resistance 2.0 - 5.0 ohm
2.0 - 5.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON JX89626 PES
LNP* STAT-KON* JX89626 is a compound based on Polyethersulfone containing Proprietary Fillers. Added feature of this material is: Electrically Conductive.
Surface Resistance 2.0 - 5.0 ohm
2.0 - 5.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON KX96321 POM
LNP* STAT-KON* KX96321 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear
LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear
LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.
Surface Resistance 2.0 - 5.0 ohm
2.0 - 5.0 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon REL36 PA 66
LNP* Stat-Kon* REL36 is a compound based on Nylon 6/6 containing carbon fiber and PTFE. Characteristics of this grade are Statically Conductive.This data was supplied by SABIC-IP for the Americas r..
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear..
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT
LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region.
Surface Resistance 2.0 - 5.0 ohm
2.0 - 5.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT
LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON WS002I PBT
LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AE002 ABS
LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON FX91304 PE
LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66
LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Surface Resistance 2.0 ohm
2.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific)
LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon MDM40 PP
LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region.