Electrical Properties Metric English Comments
Surface Resistance 1600 - 5.00e+16 ohm
1600 - 5.00e+16 ohm
Average value: 4.63e+15 ohm Grade Count:12
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Surface Resistance 1600 ohm
1600 ohm
LATI Latiohm 73-09 PD01 G/20 POM, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyoxymethylene (POM). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..