Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.64e+13 ohm | 1.64e+13 ohm | |
Arkema Group Pebax® 5533 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE(PEBA) hardness 55 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: overmolded parts for sport good (Footba.. |