Polymer Property : Surface Resistance = 1.00e+18 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 1.00e+13 - 1.00e+18 ohm
1.00e+13 - 1.00e+18 ohm
Average value: 2.50e+17 ohm Grade Count:4
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Surface Resistance 1000 - 1.00e+18 ohm
1000 - 1.00e+18 ohm
Average value: 4.11e+16 ohm Grade Count:31
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Surface Resistance 1.00e+17 - 1.00e+18 ohm
1.00e+17 - 1.00e+18 ohm
ASTM D257
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Surface Resistance 1.00e+6 - 1.00e+18 ohm
1.00e+6 - 1.00e+18 ohm
Average value: 3.58e+17 ohm Grade Count:13
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Surface Resistance 1.00e+15 - 1.00e+18 ohm
1.00e+15 - 1.00e+18 ohm
Average value: 6.80e+17 ohm Grade Count:20
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Surface Resistance 1.00e+17 - 1.00e+18 ohm
1.00e+17 - 1.00e+18 ohm
ASTM D257
Mitsui AURUM® PL450C Polyimide  (discontinued **)
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU..