Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 0.20 ohm | <= 0.20 ohm | Chomerics TM 71 |
Parker Chomerics CHO-MASK II HT Conductive Foil Tape The CHO-MASK II family of EMI foil tapes includes both Standard Tack (ST) and High Tack (HT) versions for providing a conductive, non-corroding surface on painted metal electronic enclosures. CHO-MA.. |
|||
Surface Resistance | <= 0.20 ohm | <= 0.20 ohm | Chomerics TM 71 |
Parker Chomerics CHO-MASK II ST Conductive Foil Tape The CHO-MASK II family of EMI foil tapes includes both Standard Tack (ST) and High Tack (HT) versions for providing a conductive, non-corroding surface on painted metal electronic enclosures. CHO-MA.. |