Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 0.016 ohm @Temperature 85.0 °C, Time 605000 sec |
<= 0.016 ohm @Temperature 185 °F, Time 168 hour |
(TR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCH Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |