Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 0.0090 ohm | <= 0.0090 ohm | Initial Taber Abrasion; CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |