Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.010 ohm @Temperature 35.0 °C, Time 605000 sec |
0.010 ohm @Temperature 95.0 °F, Time 168 hour |
95% RH, Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Initial; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 35.0 °C, Time 605000 sec |
0.010 ohm @Temperature 95.0 °F, Time 168 hour |
95% RH, Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Initial; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 35.0 °C, Time 605000 sec |
0.010 ohm @Temperature 95.0 °F, Time 168 hour |
95% RH, Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Initial; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 35.0 °C, Time 605000 sec |
0.010 ohm @Temperature 95.0 °F, Time 168 hour |
95% RH, Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Initial; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 - 0.015 ohm @Thickness 0.0250 mm |
0.010 - 0.015 ohm @Thickness 0.000984 in |
Printed onto 125 µm PET film |
Gwent Electronic Materials C2081126P2 Conductive Silver Polymer Paste This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electrochemical sensors and conductive tracks. It may be .. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 35.0 °C, Time 605000 sec |
0.010 ohm @Temperature 95.0 °F, Time 168 hour |
95% RH, Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Initial; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Surface Resistivity per Square | 0.010 ohm @Temperature 70.0 °C, Time 7.88e+6 sec |
0.010 ohm @Temperature 158 °F, Time 2190 hour |
Final; CHO-TM-TP57 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |