Polymer Property : Electrical Resistivity = 9.90e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 9.90e+15 ohm-cm
9.90e+15 ohm-cm
ASTM D257
Plenco 51335 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51335 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in black only.Information ..