Polymer Property : Electrical Resistivity = 7.00e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 7.00e+13 - 1.00e+15 ohm-cm
7.00e+13 - 1.00e+15 ohm-cm
Average value: 4.88e+14 ohm-cm Grade Count:6
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 7.00e+13 ohm-cm
7.00e+13 ohm-cm
Covestro Baydur® GS PIR A Polyurethane
PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015..
Electrical Resistivity 7.00e+13 ohm-cm
7.00e+13 ohm-cm
Covestro Baydur® GS PIR B Polyurethane
PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015..
Electrical Resistivity 7.00e+13 ohm-cm
7.00e+13 ohm-cm
Arkema Group Rilsan® BZM 30 TL Nylon 11, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MHL,18-050,GF30Rigid grade with glass fiber (30%) filler for injection molding. Available colors: black and natural. Light and heat stabilized.Rigidity. High compressive st..