Polymer Property : Electrical Resistivity = 4.40e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 4.40e+14 ohm-cm
4.40e+14 ohm-cm
Momentive Performance Materials RTV8262 Red General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Electrical Resistivity 4.40e+14 ohm-cm
4.40e+14 ohm-cm
Momentive Performance Materials RTV60 Red Extreme High Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..