Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1010L Polycarbonate, Unreinforced, Intermediate Flow Information provided by Ravago. |
|||
Electrical Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1017L Polycarbonate, Unreinforced, High Flow, Mold Release Information provided by Ravago. |
|||
Electrical Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Electrical Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1025L Polycarbonate, High Flow, Mold Release Information provided by Ravago |
|||
Electrical Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1032L Polycarbonate, Unreinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Electrical Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1310L Polycarbonate, UV Stabilized, Intermediate Flow, Mold Release Information provided by Entec. |
|||
Electrical Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1317L Polycarbonate, UV Stabilized, Higher Flow, Mold Release Information provided by Ravago. |
|||
Electrical Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1332L Polycarbonate, UV Stabilized, Unreinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |