Polymer Property : Electrical Resistivity = 3e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity >= 3e+11 ohm-cm

@Temperature 150 °C
>= 3e+11 ohm-cm

@Temperature 302 °F
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy
Master Bond EP112FLAO-1 is a toughened two component, high performance epoxy resin system featuring very good temperature resistance, fine thermal conductivity and electrical insulation values with ..