Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 3.00e+12 ohm-cm | 3.00e+12 ohm-cm | ASTM D257 |
Rogers Corporation Poron® 4701-50-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Electrical Resistivity | 3.00e+12 ohm-cm | 3.00e+12 ohm-cm | ASTM D257 |
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Electrical Resistivity | 3.00e+12 ohm-cm | 3.00e+12 ohm-cm | ASTM D257 |
Plenco 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 7000 is the replacement material for the former Union Carbide BMM-7000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding and preheating characteristics.. |
|||
Electrical Resistivity | 3.00e+12 - 1.00e+15 ohm-cm | 3.00e+12 - 1.00e+15 ohm-cm | Average value: 4.80e+14 ohm-cm Grade Count:16 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Electrical Resistivity | 3.00e+12 ohm-cm | 3.00e+12 ohm-cm | |
Covestro Desmopan® 588 Thermoplastic Polyurethane Desmopan 588 is a TPU on the basis of a special ether with good microbe-resistance.Applications: Cable sheathing, hoses, profiles.Information provided by Bayer.As of 1 September 2015, Bayer Material.. |
|||
Electrical Resistivity | 3.00e+12 ohm-cm | 3.00e+12 ohm-cm | |
Covestro Desmopan® 786 Thermoplastic Polyurethane Desmopan 786 is a TPU on the basis of a special carbonate with very good microbe-resistance.Applications: Tabular films, films, profiles.Information provided by Bayer.As of 1 September 2015, Bayer M.. |
|||
Electrical Resistivity | 3.00e+12 ohm-cm | 3.00e+12 ohm-cm | ASTM D257 |
Plaslok 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7000 is the replacement material for .. |
|||
Electrical Resistivity | 3.00e+12 ohm-cm | 3.00e+12 ohm-cm | ASTM D257 |
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |