Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.50e+12 - 2.50e+12 ohm-cm @Temperature 65.0 - 65.0 °C |
2.50e+12 - 2.50e+12 ohm-cm @Temperature 149 - 149 °F |
Average value: 2.50e+12 ohm-cm Grade Count:3 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 2.50e+12 ohm-cm @Temperature 65.0 °C |
2.50e+12 ohm-cm @Temperature 149 °F |
Insulation Resistance During 10th day Cycling (95% Relative Humidity) |
Cytec CC-1191 (Conap) Acrylic Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 2.50e+12 ohm-cm @Temperature 65.0 °C |
2.50e+12 ohm-cm @Temperature 149 °F |
Insulation Resistance During 10th day Cycling (95% Relative Humidity) |
Cytec CE-1170 (Conap) Acrylic Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 2.50e+12 ohm-cm @Temperature 65.0 °C |
2.50e+12 ohm-cm @Temperature 149 °F |
Insulation Resistance During 10th day Cycling (95% Relative Humidity) |
Cytec CE-1171 (Conap) Acrylic Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |