Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+8 - 1.00e+15 ohm-cm | 2.00e+8 - 1.00e+15 ohm-cm | Average value: 9.97e+13 ohm-cm Grade Count:20 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Electrical Resistivity | 2.00e+8 ohm-cm | 2.00e+8 ohm-cm | |
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite.. |