Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.80e+15 ohm-cm | 1.80e+15 ohm-cm | |
Momentive Performance Materials RTV615 Clear General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |