Polymer Property : Electrical Resistivity = 1.20e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.20e+13 ohm-cm
1.20e+13 ohm-cm
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out..
Electrical Resistivity 1.20e+13 ohm-cm
1.20e+13 ohm-cm
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas..
Electrical Resistivity 1.20e+13 ohm-cm
1.20e+13 ohm-cm
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr..